Table. 1.

Table. 1.

Flexural strength of cast resin specimens according to post-curing treatment time (unit: MPa)

NO. 5 minute 10 minute 15 minute
1 70.55 109.59 122.51
2 87.89 101.65 108.7
3 91.57 110.19 139.99
4 84.04 92.68 129.06
5 74.64 101.92 135.2
6 101.23 112.1 137.83
7 95.79 99.57 118.01
8 104.91 98.28 113.43
9 83.6 116.56 120.54
10 96.71 102.02 122.08
11 88.3 114.1 105.61
12 98.33 100.82 106.73
13 73.08 109.74 124.86
Mean±SD 88.51±11.00a 105.32±7.12b 121.89±11.46c
F=35.80, p<0.001

p-value by one-way ANOVA.

a,b,cSame letters indicate statistically indifferent by Tukey HSD Test multiple comparison.

Int J Clin Prev Dent 2024;20:170-4 https://doi.org/10.15236/ijcpd.2024.20.4.170